Parts Boiling Time?
#1
How long do I boil them for? Looking to do my wing/stay.

-Edit-

One more Q. Do I run them under cold water after, or just let them cool off to room temp?
Tekno EB48.4 HobbyWing XR8 Sanwa M12
Reply
#2
10 minutes
TEAM DENTTEK HACKING OUR WAY TO THE TOP!!!!!!

THE ANGRY PEAR IS BACK
Reply
#3
Awesome. Thanks.
Tekno EB48.4 HobbyWing XR8 Sanwa M12
Reply
#4
One more Q. Do I run them under cold water after, or just let them cool off to room temp?
Tekno EB48.4 HobbyWing XR8 Sanwa M12
Reply
#5
just turn off the stove and let them cool down
TEAM DENTTEK HACKING OUR WAY TO THE TOP!!!!!!

THE ANGRY PEAR IS BACK
Reply
#6
So...Once the 10 is up cut off heat, let sit in the pot till cool?

Or get the pot to a boil, and cut off the heat and let them sit in it for 10?
Tekno EB48.4 HobbyWing XR8 Sanwa M12
Reply
#7
boil for ten then cut the heat
TEAM DENTTEK HACKING OUR WAY TO THE TOP!!!!!!

THE ANGRY PEAR IS BACK
Reply
#8
don't let the parts sit on the bottom of the pan. they should float but watch them close
TEAM DENTTEK HACKING OUR WAY TO THE TOP!!!!!!

THE ANGRY PEAR IS BACK
Reply
#9
Has anyone tested to see if this really works?

Just curious...
Reply
#10
Lots of people have. The parts get more flexible so tollerances aren't as good (not great for racing) but they take more abuse. (better for bashing)
Reply
#11
FreeRideJunkie Wrote:Lots of people have. The parts get more flexible so tollerances aren't as good (not great for racing) but they take more abuse. (better for bashing)



Its just as good for racing as it is for anything. It doesnt majke the parts that soft... It just takes away brittleness
Dont mess wit my sig Line tune!
--Then follow the rules! haha!-- -Tune
Reply
#12
Yeah I just did it on the wing/stay and I can notice alot more flexableness in the wing...And a little more in the mount.
Tekno EB48.4 HobbyWing XR8 Sanwa M12
Reply
#13
Yeah... I didn't mean that they would just bend... It's just that if people complain about plastics bending on certain RC's too much as is and how it creates slop... boiling would only make it worse. That is why so many people go graphite on 1/10 scales. It is brittle but very hard... there are pros and cons to everything.
Reply


Possibly Related Threads…
Thread Author Replies Views Last Post
  Parts cleaning? Ultra sonic cleaner? mikeh 13 8,135 05-05-2007, 03:02 PM
Last Post: Astro
  Boiling off old tires DAVEC-NITRO-RS4 44 8,809 12-10-2006, 09:54 AM
Last Post: rocco79
  Homemade parts redzebra24 9 5,780 05-09-2006, 07:26 PM
Last Post: redzebra24

Forum Jump:


Users browsing this thread: 1 Guest(s)